T 45
Tu 52B E355
4T45
|
C |
Si |
Mn |
S |
P |
Cr |
Mo |
Ni |
|
0,17
0,25 |
0,10
0,35 |
1,30
1,70 |
≤ 0,040 |
≤ 0,040 |
≤ 0,25 |
≤ 0,10 |
≤ 0,40 |
Mechanical Characteristics:
- Supplied in the hardened and tempered
or normalised
condition.
- Rm
: 700/900 MPa
- Rp 0,2
: ≥ 620 MPa
T 60
25CrMo4 3T60
|
C |
Si |
Mn |
S |
P |
Cr |
Mo |
|
0,22
0,29 |
0,10
0,25 |
0,50
0.80 |
≤ 0,015 |
≤ 0,015 |
0,90
1.20 |
0,15
0.25 |
Mechanical Characteristics:
- Supplied in the hardened and tempered
or normalised
condition.
- Rm
: 1150/1350 MPa
- Rp 0,2
: ≥ 1050 MPa
- Elongation
: ≥ 6%